Compute the concentration of Li (in wt%) that is needed.?

Aluminum-lithium alloys have been developed by the aircraft industry to reduce the weight of an aircraft and improve the performance. A commercial aircraft skin material having a density of 2.47 g/cm^3 is desired. Compute the concentration of Li (in wt%) that is needed.